Raw Material Preparation and Compounding
Raw Material Preparation and Compounding: Select HDPE resin pellets, choosing the appropriate grade based on product requirements.
Add additives according to the formulation—such as antioxidants, UV stabilizers, masterbatches, zinc stearate (lubricant), and calcium carbonate (filler)—with dosages determined by specific requirements.
Mixing
Mixing: HDPE granules and various additives are fed into a high-speed mixer and thoroughly blended to ensure the masterbatch and additives evenly coat the surface of the granules.
The mixed material can be fed directly into the extruder hopper or pelletized prior to extrusion, depending on the complexity of the formulation.
Melt Extrusion
Melt Extrusion: HDPE sheet extrusion typically employs a single-screw extruder. The screw is divided into three sections: the feed section (conveying section), which steadily advances solid granules and provides initial compaction;
the compression section (plasticizing section), where the screw channel gradually shallows and the material begins to melt under compression and shear, transitioning from a solid state to a viscous fluid state;
and the homogenization section (metering section), which ensures uniformity in melt temperature, pressure, and composition, while establishing stable extrusion pressure.
Die Head and Die Shaping
Die Head and Die Shaping: The die head converts the rotational motion of the screw output into linear motion, ensuring uniform distribution of the melt.
Sheet extrusion utilizes a flat die (slit die); the melt is extruded from the die lips to form a continuous sheet.
Three-roll calendering, cooling, and shaping
Three-roll calendering, cooling, and shaping: After the molten sheet is extruded from the die, it immediately enters a three-roll calender (typically arranged vertically in an "I" configuration) to undergo cooling, shaping, and surface calendering.
Haul-off
Haul-off: After cooling and shaping, the sheet is pulled out at a constant speed by the haul-off unit; the haul-off speed must be precisely matched to the extrusion speed.
Excessive haul-off speed causes the sheet to thin out and fall short of the required thickness, while insufficient speed leads to material accumulation, increased thickness, and surface wrinkling.
Cutting
Cutting: Depending on product specifications, an inline cutter cuts the continuous sheet to the required length, or the material is wound into coils (suitable for thin sheets).
Post-processing and Quality Inspection
Post-processing and Quality Inspection: Natural Aging—It is recommended to let the extruded sheets sit at room temperature for at least 24 hours to relieve residual internal stress and ensure dimensional stability. Quality Inspection—Inspect for appearance (bubbles, scratches, color variations) and dimensional accuracy (thickness tolerance of ±0.2–0.3 mm); package and warehouse the product after it passes inspection.